http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103741490-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-643 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-653 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-568 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 |
filingDate | 2013-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103741490-B |
titleOfInvention | Textile shuttle-woven fabric anti tear finishing agent and preparation method |
abstract | The present invention textile shuttle-woven fabric anti tear finishing agent and preparation method, by polyethylene glycol 100 ~ 200 parts, polypropylene glycol 100 ~ 200 parts, hexamethylene diisocyanate 45 ~ 100 parts, BDO 6 ~ 16 parts, linear polyethoxy ether modified polyorganosiloxane 9 ~ 20 parts, close through pre-polymerization, aqueous solution of sodium bisulfite, after emulsification, mix composite making with the amino modified organic siloxane emulsion of hydrophilic 100 ~ 260 parts.After this finishing agent arranges, COTTON FABRIC is soft, smooth, does not reduce the original ultimate strength of fabric, and maintain the hydrophily of COTTON FABRIC itself while tearing brute force significantly promotes. |
priorityDate | 2013-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |