http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103730632-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-028 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-624 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-362 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1397 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1397 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 |
filingDate | 2013-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103730632-B |
titleOfInvention | A kind of based on diatomaceous lithium sulfur battery anode material and methods for making and using same thereof |
abstract | The invention discloses a kind of based on diatomaceous lithium sulfur battery anode material and methods for making and using same thereof, this positive electrode take diatomite as skeleton, elemental sulfur is injected diatomite to obtain carrying a sulphur composite material, then it is coated to carry out conductive materials to this year sulphur composite material.Utilize diatomite effectively can reduce the dissolving of polysulfide and the volumetric expansion suppressing sulphur in charge and discharge process, improve the cycle performance of lithium-sulfur cell.The coated conductivity enhancing material of conductive materials, improves the capacity of lithium-sulfur cell.Preparation technology of the present invention is simple, and diatomite belongs to natural environment-friendly materials, with low cost, is beneficial to lithium-sulfur cell industrialization.Meanwhile, diatomaceous introducing has also promoted industrial transformation and the upgrading of nonmetallic mineral. |
priorityDate | 2013-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |