http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103725231-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9a667348209b362e68982a579024a210 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-10 |
filingDate | 2013-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e168bf6a3a175938184aeab32f53e979 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_885319476ab15a39b0844ba0e6da0386 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e6c3e5a0d88c6b9411db5de4be63374d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3ff9952aa89fc9c15bd845b4dd500471 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a1d68bb62155ead8be15a561aa6dd8f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ca92e27f4f06b7c83b0233654182d0eb |
publicationDate | 2015-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103725231-B |
titleOfInvention | Adhesive material for adhesive tapes and preparation method thereof |
abstract | The invention discloses an adhesive material for adhesive tapes. The invention is characterized in that the adhesive material is prepared by mixing 1000 parts by mass of acrylate prepolymer resin with the solid content of 40%, 3-10 parts by mass of curing agent and 200-500 parts by mass of diluting solvent. The preparation method of the acrylate prepolymer resin comprises the following steps: adding 350 parts of butyl acrylate, 150-200 parts of 2-ethylhexyl acrylate, 250-350 parts of ethyl methacrylate, 200-300 parts of functional monomer, 100-150 parts of glycidyl methacrylate, 1200 parts of solvent and 8-20 parts of initiator into a reaction kettle, and stirring and mixing; and in a nitrogen protective atmosphere, heating to 70-75 DEG C to react for 4-6 hours, and adding a solvent until the solid content reaches 40%. The adhesive material for adhesive tapes has the advantages of high heat resistance, high aging resistance, high working properties and favorable product performance, is convenient to use, and can be used for manufacturing various single-sided and double-sided pressure-sensitive adhesive tapes and optical clear adhesive tapes. |
priorityDate | 2013-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |