http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103725217-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L35-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 |
filingDate | 2013-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103725217-B |
titleOfInvention | A kind of Resin material protective layer |
abstract | The object of the invention is at mould molding temperature (generally more than 80 DEG C, common is 100 DEG C ~ 120 DEG C) and obstruction or bonding can not be produced, the thermoplastic resin protective layer that molding shrinkage is low.Described Resin material protective layer, comprises the tack coat of outer field protective layer and internal layer, and its skin can be single or composite bed, skin comprises following component, first part: vinyl-α, β-unsaturated fatty acids and α, the interpolymer of β-unsaturated fatty acid ester, 60 ~ 90 parts; Second section: with alhpa olefin, glycidyl acrylate, ethene acid esters is the terpolymers 1 ~ 5 part of monomer; Part III: polyethylene 15 ~ 30 parts.Vinyl-α in described first part, β-unsaturated fatty acids proportion is 10% ~ 15%. |
priorityDate | 2013-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 25.