http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103722179-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-24 |
filingDate | 2013-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103722179-B |
titleOfInvention | For the preparation method of the nano copper slurry of electrically conductive ink |
abstract | The present invention relates to a kind of preparation method of the nano copper slurry for electrically conductive ink.This preparation method being used for the nano copper slurry of electrically conductive ink comprises Jiang Tongyuan and adds in solvent, even in stirred at ambient temperature, obtains copper source dispersion liquid; Dispersant is added in the dispersion liquid of described copper source, even in stirred at ambient temperature, obtain the first mixed liquor; Complexing agent is added in described first mixed liquor, even in stirred at ambient temperature, obtain the second mixed liquor; In described second mixed liquor, add reducing agent, react 30 minutes ~ 3 hours under room temperature, obtain nano copper colloid; And described in obtaining after being concentrated by described nano copper colloid, be used for the step of the nano copper slurry of electrically conductive ink.The method preparation technology is simple, and Nanometer Copper is difficult to oxidized, and the dispersiveness of Nanometer Copper is better. |
priorityDate | 2013-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.