http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103694585-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ce634486f59ddde55841f447c220fa70 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
filingDate | 2013-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_082ca1131a236b632a2416b513debb6f |
publicationDate | 2014-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103694585-A |
titleOfInvention | Preparation method of special imitated ABS (acrylonitrile butadiene styrene) highlight material |
abstract | The invention provides a preparation method of a special imitated ABS (acrylonitrile butadiene styrene) highlight material. A formula comprises the following components: AS (acetosyringone), ABS with high melt index, PC (polycarbonate), a compatilizer, rubber powder, auxiliaries and black masterbatch, wherein the mass fraction of the rubber powder is 10%-15%, and the mass fraction of the compatilizer is 3%-5%. Material drying by a drying machine is added in pretreatment, a No. 35 machine is adopted as an extruder, a 200-litre high-speed mixer is adopted for material mixing, and a 168T sample board machine is adopted as an injection molding machine, so that the processing fluidity and rigidity of a product are improved. |