http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103633392-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-52 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G45-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-54 |
filingDate | 2013-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103633392-B |
titleOfInvention | A kind of method being prepared nickel manganese hydroxide by waste and old electrokinetic cell directed circulation |
abstract | The invention belongs to nickel manganese hydroxide preparing technical field, disclose a kind of methods and applications being prepared nickel manganese hydroxide by waste and old electrokinetic cell directed circulation.The method comprises following concrete operations: disassemble waste nickel lithium manganate power battery, is separated positive plate and negative plate; Positive plate is broken, heating, screening, oversize is aluminium foil, and screenings is nickel lithium manganate cathode material powder and acetylene black; Acid adding in screenings, crosses and filters acetylene black, obtain mixed solution that is nickeliferous, manganese; Add nickel source, manganese source and excipient successively; Regulate pH, add nucleation-accelerant, heating for dissolving, microwave reaction; Cooling, filtration, washing, drying, obtain nickel manganese hydroxide.The present invention utilizes nucleation-accelerant to form nickel manganese hydroxide nucleus, and connect nucleus by excipient, obtain dandelion shape particle, uniform particle sizes, appearance structure is consistent, and growth in order.Utilize it as positive electrode, the battery that specific capacity significantly improves can be prepared. |
priorityDate | 2013-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 65.