http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103614199-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cdf314cbe90397243e0ac6ff3c1acb40 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10N40-32 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10M177-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10M169-06 |
filingDate | 2013-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f60195acf48f0a7cf62ac5c48e2e9689 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_222e5937580790bd4ab2395ecaf3fd28 |
publicationDate | 2015-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103614199-B |
titleOfInvention | Preparation method of maintenance agent for lubricating and protecting wire rope |
abstract | The invention relates to a preparation method of a maintenance agent for lubricating and protecting a wire rope, which comprises the following steps: 1) heating base oil and base grease to 80-90 DEG C, and uniformly mixing; 2) sequentially adding an antioxidant, a rust inhibitor, colloidal graphite, nano molybdenum disulfide and a thickener into the mixed solution obtained in the step 1), stirring uniformly, and keeping the temperature at 80-90 DEG C; and 3) when the material obtained in the step 2) is cooled to 80 DEG C below, carrying out homogeneization treatment with a triple-roller mill to obtain the wire rope maintenance agent. The wire rope maintenance agent has the advantages of favorable high/low temperature properties, favorable extreme pressure property, high rust resistance and high corrosion resistance. |