titleOfInvention | The Biological desiliconization method of vanadium titano-magnetite |
abstract | The invention belongs to field of ore extraction, the biological desiliconization relating to a kind of vanadium titano-magnetite, with the method for enriched iron, titanium valuable element, is specifically related to the cultivation of silicate bacteria and the treatment process of mineral.The present inventor is in order to realize the biological desiliconization of vanadium titano-magnetite, silicate bacteria is obtained from commercial undertaking, utilize v-ti magnetite breeze to mix Alexandria sieve husband substratum to cultivate it, the silicate bacteria after cultivation is more conducive to the silicon removed in vanadium titano-magnetite.Step is as follows: A, cultivation silicate bacteria: B, pulverizing vanadium titano-magnetite are to crossing 40-400 mesh sieve; C, biological desiliconization.Silicate bacteria is still comparatively obvious to the immersion Zn of silicon in vanadium titano-magnetite. |