http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103547450-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D2565-383 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H19-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H27-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-10 |
filingDate | 2012-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103547450-B |
titleOfInvention | There is paper and the cardboard packaging of polymeric blends barrier coat |
abstract | Describe a kind of paper or the cardboard packaging that comprise the recovery paper being exposed to mineral oil, the barrier layer that described packaging has the aqueous polymer dispersion by applying to comprise the mixture of at least two kinds of polymer A and B and obtains.Polymer A is by emulsion polymerisation (methyl) acrylic acid Cn 1 -Cn 4 arrcostab, acid monomers as acrylic or methacrylic acid, 0-20 % by weight acrylonitrile and other monomers of 0-10 % by weight and prepare, wherein the glass transition temperature of copolymer A higher than+45 DEG C and the glass transition temperature of polymer B lower than+10 DEG C.The mean value calculated by the glass transition temperature of each polymer is+10 DEG C to+45 DEG C.Described barrier layer can be positioned on a surface of package, or can form in multiple layers of multi-layer packaging coating, or can be used as coating and be positioned on the side of the bag of packaging. |
priorityDate | 2011-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 102.