http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103531748-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-602 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1399 |
filingDate | 2012-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103531748-B |
titleOfInvention | The preparation method of active material of lithium ion battery electrode |
abstract | The invention provides a kind of preparation method of active material of lithium ion battery electrode, it comprises: mixed with polyacrylonitrile by elemental sulfur, forms a mixture; In vacuum or protective atmosphere, 250 DEG C to 500 DEG C temperature ranges heat this mixture, obtain a S-containing composite; And reacted with the reducing agent of elemental sulfur in liquid phase medium by this S-containing composite, thus part removes the sulphur in this S-containing composite, obtains sulfuration polypyrrole pyridine. |
priorityDate | 2012-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |