http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103525319-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6f6335a08675e249951c052b04706eb0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J151-06 |
filingDate | 2013-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f81624bbd4f890389d5a8c46f02faf58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3fd169ae1b44948a47c1f33a50d67a4b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c43125818455755557dcd437c380606 |
publicationDate | 2015-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103525319-B |
titleOfInvention | Ultraviolet crosslinking and curing EVA (ethylene vinyl acetate copolymer) optical adhesive film and preparation method thereof |
abstract | The invention relates to an ultraviolet crosslinking and curing EVA (ethylene vinyl acetate copolymer) optical adhesive film and a preparation method thereof. The ultraviolet crosslinking and curing EVA optical adhesive film takes EVA or a mixture of the EVA and an EVA-modified graft polymer as a base material; in the mixture, the weight ratio of the EVA to the EVA-modified graft polymer is 1: 0-0.2; and according to 100 parts of the of the base material by total weight, the EVA optical adhesive film further comprises the following raw materials in part by weight: 0.1-5 parts of photoinitiator, 0.1-5 parts of multifunctional crosslinking agent, 0.1-1 part of antioxidant, 0.1-1 part of light stabilizer, 0.1-2 parts of coupling agent and 0.1-10 parts of bonding resin. The preparation method is short in operating time, small in required equipment investment, simple in process, convenient in operation and maintenance, energy-saving, environment-friendly and high in production efficiency; the production cost is reduced; the ultraviolet crosslinking and curing EVA optical adhesive film is low in defective ratio and excellent in mechanical properties; and during use, the ultraviolet crosslinking and curing EVA optical adhesive film can be crosslinked and adhered through radiation of specific ultraviolet, so that optical adhesive OCA and liquid optical adhesive LOCA for adhering a display in the traditional electronic industry can be replaced. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I614222-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017088487-A |
priorityDate | 2013-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 106.