classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-00 |
filingDate | 2013-10-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103524773-B |
titleOfInvention | The surface treatment method of fluoropolymer polymer working of plastics and method of attachment |
abstract | The surface treatment method that the invention discloses a kind of fluoropolymer polymer working of plastics, comprises step: (1) is used trichloro-ethylene solution to clean described working of plastics natural drying in air; (2) described working of plastics is immersed in to 15~20min in solution A; In described solution A, calculate by weight, comprise 1000~1200 parts of thiophene, 150~200 part 1,2-benzanthracene, 50~100 parts of SODIUM METALs; Then use washed with de-ionized water, re-use the hot-air seasoning of 30~40 DEG C; (3) described working of plastics being immersed in to concentration is 5~10min in 50~70% phosphoric acid solution; Then use washed with de-ionized water, re-use the hot-air seasoning of 30~40 DEG C. The invention also discloses a kind of method of attachment that adopts adhesive to bond to fluoropolymer polymer working of plastics, comprise the step of aforesaid surface treatment method. |