http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103483656-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_913177f4080a60976a343ed39e534dcb |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B17-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L3-04 |
filingDate | 2013-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5341dbaa5287bf62e0e20eb191eaca79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fa34c3a44b9cd7f376866109aee65b0a |
publicationDate | 2015-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103483656-B |
titleOfInvention | Reprocessing method for waste rubber |
abstract | The invention belongs to the field of machine manufacturing, and particularly relates to a reprocessing method for waste rubber. The waste rubber is subjected to seven steps of treatment including smashing, cleaning, melting, modifying, vacuum defoaming, shape forming and vulcanizing. An oxygen plasma activated carbon tube, modified starch and pigment are added and stirred uniformly with rubber cement to realize modification, wherein the content of the oxygen plasma activated carbon tube is 1-5%, and the content of the modified starch is 3-8%. In the shape forming process, a mixture of magnesium-aluminium hydrotalcite, ammonium polyphosphate and magnesium hydroxide are added, wherein the ratio of the magnesium-aluminium hydrotalcite to the ammonium polyphosphate to the magnesium hydroxide in the mixture is 2:1:2. After the waste rubber is subjected to the series of treatment, waste is turned into wealth, used rubber is purified, and the ductility, oxidation resistance and fire resistance of reproduced rubber are improved. |