titleOfInvention | A kind of Graphene-copper oxide three-dimensional foam composite material |
abstract | The present invention discloses a kind of preparation method of Graphene-copper oxide three-dimensional foam composite material, comprises the following steps: step one, material oxidation Graphene and mantoquita is mixed than soluble in water by certain mass; Step 2, graphene oxide to be separated by centrifugal or suction filtration by the liquid mixed in step one, and with water or alcohol washes clean; Step 3, the product obtained in step 2 is re-dispersed in the aqueous solution, subsequently product is carried out lyophilize process; Step 4, by step 3 obtain product thermal treatment under air or oxygen obtain Graphene-copper oxide three-dimensional foam composite material, wherein said thermal treatment temp is at 150-800 degree Celsius, and heat treatment time was at 10 seconds-10 hours. |