http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103476831-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2110-0008 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6677 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4072 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4866 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4845 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4841 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-2663 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-2648 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60N2-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-10 |
filingDate | 2012-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103476831-B |
titleOfInvention | PPG and the manufacture method of flexible polyurethane foams and seat |
abstract | The decline of the mechanical property of the foam that present invention suppression causes because of the polyol systems liquid after using storage.PPG (A1) is used to prepare polyol systems liquid, and use this polyol systems liquid to manufacture flexible polyurethane foams, this PPG (A1) be the average hydroxyl number obtained by following operation be 2~8, hydroxyl value is the PPG (A1) of 5~45mgKOH/g: through making alkylene oxide ring opening polyaddition obtain middle polyalcohol in the operation of initiator in the presence of composition metal cyanide complex catalyst, use alkali-metal hydroxide as polymerization catalyst, make oxirane to obtain in described middle polyalcohol relative to the amount ring opening polyaddition that every 1 mole initiator is 1~23 mole. |