http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103467314-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C215-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-755 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C213-02 |
filingDate | 2013-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103467314-B |
titleOfInvention | The method of a kind of nano nickel/copper composite catalyst shortening p-nitrophenol |
abstract | The present invention relates to the method for a kind of nano nickel/copper composite catalyst shortening p-nitrophenol, belong to nano-catalytic field.Carrying out according to following step: with p-NP, dehydrated alcohol for raw material, adopt nano nickel/copper composition as catalyzer, does is catalyst levels 0.5-5? wt%, 0.8? MPaHn 2 under pressure, temperature of reaction is made to be warming up to 80-160? DEG C, and insulation reaction 2-8? h.After reaction terminates, leach catalyzer, obtain high purity p-aminophenol.Nano nickel prepared by the present invention/copper composite catalyst is spheroidal particle, and consumption is few, has high catalytic activity and stability.The method processing requirement is simple, is applicable to industrial requirement. |
priorityDate | 2013-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 41.