http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103467129-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c42baed8f638fbf4f93bcbeee153962b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B38-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-08 |
filingDate | 2013-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02322032d91b5f9a05bd99a3442436b1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f0630ff566f94977824bdbdcab67108 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f886bf7331d6628631ab6390692a76cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d600633b4ffb8e7a204e40970c2f3ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b449400de13a92a0dfa73d2aaddb3af http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_498d51651a13921c1a3b75eae06b9544 |
publicationDate | 2014-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103467129-B |
titleOfInvention | Preparation process and application of foamed mine filling material containing lead and zinc smelting slag |
abstract | The invention discloses a preparation process and an application of a foamed mine filling material containing lead and zinc smelting slag. The preparation process and the application are characterized in that a stabilizer is added in the lead and zinc smelting slag to enable harmful ions in the slag to be transformed into the stable state of original minerals, industrial slag is taken as a binding material, and no alkali-activator is added, so that the foamed mine filling material is prepared. The preparation process and the application can not only treat the lead and zinc smelting slag, but also fill the mine. The process has the advantages that the harmless ions leaching rate is low, the process is simple, the cost is low, and raw materials are easy to get. |
priorityDate | 2013-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 60.