http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103450834-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_85b5a068620c47a3df374a09a97ffd92 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J109-02 |
filingDate | 2013-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c73ad92494f0b54ae1c3103d335accb |
publicationDate | 2015-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103450834-B |
titleOfInvention | Metal adhesive and preparation method thereof |
abstract | The invention discloses a metal adhesive and a preparation method thereof. The metal adhesive comprises the following components in parts by weight: 8-15 parts of dibutyl phthalate, 10-20 parts of phenyldimethylamine, 10-20 parts of talcum powder, 0.5-2 parts of triethylenetetramine, 5-12 parts of liquid nitrile-butadiene rubber and 80-100 parts of epoxy resin. The preparation method comprises the following steps: mixing the components, sufficiently stirring uniformly at 50-60 DEG C, heating the system to 75-85 DEG C, and reacting for 3-5 hours. The metal adhesive disclosed by the invention can still keep favorable shear strength and peel strength at low temperature, and can be well applied to a low-temperature environment. |