http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103450527-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-02 |
filingDate | 2013-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-01-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-01-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103450527-B |
titleOfInvention | A kind of clutch surface dipping uses anticorrosive rubber slurry |
abstract | The invention discloses a kind of clutch surface dipping and use anticorrosive rubber slurry, it is obtained by the raw material of following weight parts: trioctyl trimellitate 0.5-0.8, clorafin 0.2-0.4, steel fiber 0.2-0.4, Resorcinol 0.2-0.4, sodium carbonate 0.3-0.5, SULPHUR POWDER 4-6, molybdenumdisulphide 0.1-0.2, altax? 0.6-1.0, Vulcanization accelerator TMTD? 0.2-0.4, stearic acid 0.7-1, carbon black 7-9, graphite 5-8, modified filler 25-30, zinc oxide 7-9, resol 7-9, magnesium naphthenate 1-2, barium sulfate 2-4, antioxidant 264? 0.1-0.2, styrene-butadiene rubber(SBR) 8-10, paracril 6-8, dimethylbenzene is appropriate. |
priorityDate | 2013-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |