http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103436983-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_87fc794fb90eaed3227b9cb9b5d91f26 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-94 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 |
filingDate | 2013-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b1927de6e303060e221fd79bf3997a94 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d4413b8294f1aaca75051b0b09046ec http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9a1a76959395d47ccc854e3b1fed1280 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_623725c6738451778d41959a5d078049 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8fac486a317112fe401546cff6b74c8c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc8e188abc27ef4ff7edd816a5fe1a50 |
publicationDate | 2015-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103436983-B |
titleOfInvention | High-resilience urethane elastic fiber as well as preparation method thereof |
abstract | The invention relates to a preparation method of a high-resilience urethane elastic fiber. The preparation method comprises the following steps: (1) mixing raw materials, namely, polytetramethylene ether glycol (PTMEG) and 4, 4-diphenylmethane diisocyanate (MDI) to carry out reaction so as to obtain a prepolymer; (2) adding a certain amount of a mixed diamine chain extender into the prepolymer to form polymer liquor; (3) quickly adding polyamine (the number of functional groups is greater than 2) into the polymer liquor while stirring to carry out reaction so as to form polyurethaneurea liquor; (5) carrying out reaction on MDI and polyether polyhydric alcohol and blocking with ethanediamine to prepare oligomers; (6) blending nano attapulgite with the oligomers to prepare a prepreg; and (7) mixing the polyurethaneurea liquor with the prepreg to prepare a spinning dope, and spinning to form the high-resilience urethane elastic fiber. The preparation method of the high-resilience urethane elastic fiber provided by the invention satisfies the demands on the high-resilience urethane elastic fiber in certain special fields, and the resilience of the urethane elastic fiber is improved. |