titleOfInvention | A kind of Environment-friendlyhigh-strength high-strength mildew-proof putty powder |
abstract | The invention provides a kind of Environment-friendlyhigh-strength high-strength mildew-proof putty powder, comprise the component of following weight percent: water-ground limestone 70-99%, grey calcium 0-30%, starch alkenyl succinate ester 0.5-10%, Vltra tears 0.2-5%, treated starch 0.5-10%, the weight percent sum of above-mentioned each component is 100%; The cohesive strength of this putty powder is strong, and mildew resistance is improved greatly, has not dry linting, non-scale, does not chap, and does not play mould advantage, and easy construction. |