classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F120-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-28 |
filingDate | 2013-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103408693-B |
titleOfInvention | The preparation method of the temperature-sensitive hydrogel that a kind of response temperature is adjustable |
abstract | The present invention relates to the preparation method of the adjustable temperature-sensitive hydrogel of a kind of response temperature, comprising: be polymerized at 0-50 DEG C by hydrogel pre-polymerization liquid, polymerization time is 1-48 hour; The component of described hydrogel pre-polymerization liquid comprises: comonomer, linking agent, initiator, catalyzer and deionized water.The inventive method is simple, and cost is lower, and material choice scope is large, the three-dimensional net structure of obtained temperature-sensitive hydrogel is even, excellent in mechanical performance, and its response temperature can in 25-90 DEG C accuracy controlling, this kind of temperature-sensitive hydrogel has wide application space in intelligent material. |