titleOfInvention | A kind of preparation method of glass fiber floor provided |
abstract | The invention belongs to manufacturing technology field, floor, be specifically related to a kind of preparation method adopting the discarded glass of recovery to be combined the glass fiber floor provided manufactured with decorative panel.Comprise the following steps: decorative panel is positioned over bottom and is provided with the bottom of the grooved mould one of fixture and fixes by (1); (2) in grooved mould one, add glass fibre and resin and make both fully mixing, crystallization obtains the floor base plate slab of bottom surface with described decorative panel; (3) taken out from described grooved mould one by floor base plate slab, turn-over is placed in grooved mould two bottom center and is fixed; (4) in grooved mould two, add glass fibre and resin and make both fully mixing, crystallization obtains the floor slab accompanying decorative panel; (5) floor slab is taken out from described grooved mould two, then carry out following process and obtain finished product floor.The glass fiber floor provided hardness that this method is produced is high, toughness foot, not easy to crack, can carry out arbitrarily cutting fluting and not peel off. |
priorityDate | 2013-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |