titleOfInvention | Emulation copper coating and production technique thereof |
abstract | The present invention relates to building and ornament materials and applied technical field.The invention provides emulation copper coating, by weight, be made up of following raw materials according: mixed solvent 670-700 part, cellulose acetate butyrate 60-70 part, vibrin 60-70 part, nitro-cotton 40-50 part, aminoresin 30-40 part, flow agent 2-5 part, anti-settling agent 25-35 part, pearly pigment 55-75 part, toner pigment 10-30 part.The present invention also provides the production technique preparing above-mentioned emulation copper coating simultaneously, step is as follows: add in cylinder by mixed solvent, cellulose acetate butyrate, vibrin, nitro-cotton, aminoresin, flow agent, anti-settling agent, pearly pigment and toner pigment successively, mixing and stirring.The present invention by introducing the directed auxiliary agent of high glass transition temperature, and selects multiple pearly pigment, is mixed, make its film reach the object of perfect reproduction copper material effect and metal-like by certain proportion. |
priorityDate | 2013-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 39.