titleOfInvention | Prepare the method for high permeability Graphene |
abstract | The present invention relates to a kind of method of preparing high permeability Graphene: step 1: utilize chemical vapour deposition technique at the uniform Graphene of Grown; Step 2: apply one deck or a uniform adhesive in destination carrier, have the one side of Graphene to be laid in destination carrier substrate length; Step 3: cover substrate top surface, adhesive is extruded and forms uniform the first adhesive phase; Step 4: remove substrate, obtain shifting the destination carrier that has Graphene, bondd by the first adhesive phase between Graphene and destination carrier; Step 5: the Graphene surface in step 4 applies uniform the second adhesive phase of one deck; Step 6: cover again the photic zone that one deck is made with transparent material on the second adhesive phase. By increasing adhesive phase, make to shift after Graphene, destination carrier is combined with Graphene firmly; In addition, by increasing photic zone, make to shift rear Graphene surface and protected, and visual effect is more clear. |