titleOfInvention | Rosin emulsion-type sizing agent, its manufacture method and paper |
abstract | The present invention relates to rosin emulsion-type sizing agent, its manufacture method and paper.The present invention provides stability and sizing excellent and be used as the rosin emulsion-type sizing agent for being emulsified material using the rosin without fortified rosin.The present invention uses a kind of rosin emulsion-type sizing agent, contain copolymer (A) and rosin (B), the copolymer (A) by the polymeric composition (a) at least containing hydrophobic monomer (a1) and monomer (a2) with anionic property functional group with (the use molal quantity with the monomer (a2) of anionic property functional group) × (valence mumber for the anionic property functional group contained in the monomer (a2) with anionic property functional group)/(use molal quantity of hydrophobic monomer (a1)) for 1.0~3.5 by way of use and obtain, pine gum (b1) of the rosin (B) at least containing 30~100 weight % and without fortified rosin. |