http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103304831-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ff21c04d0c133031ba16fefe47e1cb1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 |
filingDate | 2013-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0c0fdfba5d2205a19f6e0fa2a13b5371 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6d3ec74697ffb9edc725e0af34acbb7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ebdaf49641ec0f24820cae13b960c3fc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81cd96f001f400eb839bd24e1742413b |
publicationDate | 2014-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103304831-B |
titleOfInvention | Environment-friendly wallpaper with diatomite as substrate filler and coating slurry and preparation method |
abstract | The invention discloses environment-friendly wallpaper with diatomite as substrate filler and coating slurry and a preparation method. The diatomite substrate comprises the following components in parts by weight: 70-80 parts of modified diatomite, 20-30 parts of polyolefin, 0.03-0.15 part of heat stabilizer, 0.1-0.5 part of drying agent and 0.1-0.5 part of foaming agent. The coating slurry comprises the following components in parts by weight: 30-60 parts of deionized water, 20-30 parts of water-based latex, 20-40 parts of diatomite, 0.1-0.5 part of dispersing agent, 0.1-0.5 part of defoaming agent and 0.1-0.5 part of thickening agent. The preparation method comprises the steps of (1) preparing the modified diatomite; (2) preparing substrate granules; (3) forming the substrate of the environment-friendly wallpaper; (4) preparing diatomite dispersion liquid; (5) preparing the coating slurry of the environment-friendly wallpaper; and (6) preparing the environment-friendly wallpaper. The obtained environment-friendly wallpaper has the characteristics of low carbon, environment friendliness, strong humidity control capacity and the like. |
priorityDate | 2013-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 89.