http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103296281-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 |
filingDate | 2013-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103296281-B |
titleOfInvention | A kind of method utilizing useless positive active material to prepare plumbic acid barium circulating and recovering |
abstract | The invention discloses a kind of method utilizing useless positive active material to prepare barium cuprate circulating and recovering, (1) measures useless positive active material oxidizability, calculates lead tolerance in useless positive active material; (2) brium carbonate and useless positive active material is got in proportion, fully grinding, mixing; (3) black product plumbic acid barium will be reacted to obtain under gained mixture at a certain temperature air atmosphere; (4) gained plumbic acid barium is ground, sieve by technology, after sieving, add reuse in the lead powder preparing anode diachylon in proportion.The useless positive active material produced in lead-acid storage battery production process transforms and is prepared into plumbic acid barium by the present invention, is back to use in lead-acid storage battery production and goes, and cost-saving, reduction is polluted, turned waste into wealth, and advances the progress of the recycle utilization of lead acid accumulator. |