http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103265859-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D171-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D177-00 |
filingDate | 2013-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103265859-B |
titleOfInvention | A kind of high light transmittance coating and preparation method thereof |
abstract | The present invention relates to a kind of high light transmittance coating, its feedstock portions formula is composed of the following components by weight percentage: polyether block polyamides copolymer 1 0-13%, thermoplastic polyester elastomer 10-13%, thermoplastic polyurethane 10-13%, water soluble acrylic resin 36-47%, Trisodium Citrate 13%-20%, zinc sulfate 10-15%, nano aluminium oxide 8-10%; Described coating also comprises by dispersion agent, lubricant, the auxiliary material part of biological preservative composition; The TVOC value of described Water-soluble environment-friendlyanticorrosive preservative property coating is 0g/l, and burst size of methanal is 0g/l.Both environmental protection, has again good preservative effect. |
priorityDate | 2013-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links