http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103212367-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4c0ed78c4d5c4951a22374d61ea1f178 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-28 |
filingDate | 2013-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5683e4585f63a0285c30d83e3050cd36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_47261620eb2adf67187f9d2ccd100f29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_19e2ef40937b3cffaaefdf72dd34ee57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d6fc2f92f4ca2b172df79789b1be157d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c8bc18e73fccbaf89f8de4029a444259 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dbae042d0cbcf98d3595ef84cd11559e |
publicationDate | 2015-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103212367-B |
titleOfInvention | Method for preparing binary oxide modified diatomite powder through recycled waste WC-TiC (wolfram carbide-titanium carbide) alloy |
abstract | The invention discloses a method for preparing binary oxide modified diatomite powder through recycled waste WC-TiC alloy, and belongs to the technical field of water treatment. Firstly, alloy blocks and diatomite are subjected to pretreatment; then mixed solution of the alloy blocks, concentrated nitric acid, hydrogen peroxide and hydrofluoric acid is subjected to hydrothermal reaction; after washing, filtering and drying are performed to the mixed solution, WO3-TiO2 nano-composite particles are obtained, then the WO3-TiO2 nano-composite particles and pretreated diatomite are subjected to ultrasonic immersing loading for 12 to 24h under the effect of adjuvant, and after washing, filtering, drying and calcining are performed to the WO3-TiO2 nano-composite particles and pretreated diatomite, the WO3-TiO2 nano-composite particles and pretreated diatomite can be used for degrading organic wastewater. The WO3-TiO2 modified diatomite powder has excellent light degradation, adsorption property and reutilization property. |