titleOfInvention | Anticorrosive additive of polyaniline-coated gas phase nano silicon-dioxide and its preparation method and application |
abstract | The invention belongs to paint field, be specifically related to a kind of preparation method and application thereof of anticorrosive additive of polyaniline-coated nano-gas-phase nano silicon.Described anticorrosive additive has nucleocapsid structure, core is nano level silica dioxide granule, shell is polyaniline, polyaniline is even at the coated thickness of gas phase nano silica particles, and in the total mass of anticorrosive additive, the content of polyaniline is 9wt% ~ 50 wt%, and the specific conductivity of this anticorrosive additive reaches 10n -1 scmn -1 .The preparation method of described anticorrosive additive, comprises the following steps: that aniline monomer adheres in advance, polyreaction, aftertreatment, goes doping, adulterates.Present invention includes a kind of preparation of polyaniline-coated gas phase nano silicon-dioxide protective system, in addition baking processing after the protective system obtained spraying, can obtain the corrosion protection coating of very dense uniform, effectively protect metal. |