http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103194820-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ae36d84ea4af395b8f5b7a4d46ec880 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F11-06 |
filingDate | 2013-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fcab5c01322b49bb41168b98d13d5c45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0d7662ed8b470c71c81d385d70c5d580 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_06bbf2355bff4d9edfab859f81f14e84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c132bbf0b450eea851a5a3ce1456f8b5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7fabc180f7d7fc5b8c6cd0385f7d6899 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9a9c999d1e69f38815b32e16e76b8e8e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ae37103c2b5d0f30cf5a266f630f6c4 |
publicationDate | 2014-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103194820-B |
titleOfInvention | Method for preparing micro-nanofiber through solvent curing type electrostatic spinning |
abstract | The invention belongs to the field of a micro-nanofiber material preparation technology, and relates to a method for preparing micro-nanofiber through solvent curing type electrostatic spinning. The method comprises the following three steps of: blending a spinning solution, installing an electrostatic spinning device and preparing micro-nanofiber, specifically, blending a polymethyl methacrylate solution as the spinning solution; installing the electrostatic spinning device: sleeving a stainless steel needle head with an injector, placing the blended spinning solution in the injector, then placing the injector on a booster, enabling an anode of a high-voltage power supply to be electrically connected with the stainless steel needle head and a cathode of the high-voltage power supply to be electrically connected with a metal collecting electrode, and regulating the distance from the stainless steel needle head to the metal collecting electrode; and switching on the high-voltage power supply, producing electric spinning fiber under the action of field stress and depositing the electric spinning fiber on the metal collecting electrode. The method is simple, reliable in principle, simple and convenient to operate, strong in practicability, fast in speed, high in raw material utilization ratio and environment-friendly. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020120798-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3666940-A1 |
priorityDate | 2013-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 30.