http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103172016-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6a6f422b091ba12ea61d4adbf1b0e8e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B81C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 |
filingDate | 2013-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_635a8e6e38ff14315e9c54a2b26a7351 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9eb28443c5c4863b1e511bc4891e328 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ded9d29686319f2dc3598df4ccb18532 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fe2f3f8f4d0be427c03060b1c7e21d42 |
publicationDate | 2013-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103172016-A |
titleOfInvention | Preparation method of zinc oxide nano-wire pattern |
abstract | The invention discloses a preparation method of a zinc oxide nano-wire pattern. The method comprises the steps that: (1) a through-type polymer ordered porous membrane is prepared; (2) the through-type polymer ordered porous membrane is covered on the surface of a substrate with an zinc oxide seed layer pre-produced with a radio-frequency magnetron sputtering technology; (3) the substrate is placed into a water solution of a zinc oxide precursor and Lewis base, and is allowed to grow for a certain period of time; (4) the substrate is soaked in a mold release agent; the through-type polymer ordered porous membrane is removed; and after washing, the zinc oxide nano-wire pattern is formed on the surface of the substrate. The method provided by the invention is not dependant on existing patterning technologies such as photolithography and electron beam lithography. One-dimensional vertical orientation of the zinc oxide nano-wire pattern is high. With the method, array dimension dynamical controllable adjustment can be realized. The cost is low, and the method is simple and convenient. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103979601-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103937773-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107414071-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107598177-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103979601-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107598177-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105911033-A |
priorityDate | 2013-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |