http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103158309-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06F3-041 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-18 |
filingDate | 2012-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103158309-B |
titleOfInvention | Hard coating film, transparent conductive laminate and touch panel |
abstract | The object of this invention is to provide and there is excellent hardness and can effectively prevent curling hard coating film, transparent conductive laminate and touch panel.Hard coating film of the present invention comprises: plastic transparent substrate layer; First hard conating, is formed at the side, a face of substrate layer; Second hard conating, is formed at the side, a face of the first hard conating; 3rd hard conating, is formed at another side, face of substrate layer; And high refractive index layer, be formed at another side, face of the 3rd hard conating, the thickness of the first hard conating and the 3rd hard conating is 20 μm ~ 100 μm, the thickness of the second hard conating is 1 μm ~ 10 μm, the pencil hardness of the first hard conating and the 3rd hard conating is F ~ 2H, and the glass transition temperature of the first hard conating and the 3rd hard conating is more than 160 DEG C. |
priorityDate | 2011-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |