http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103144178-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d8b4fea93d3bc821dfb3cee1094dbf08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27D1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27M3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J189-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04F15-04 |
filingDate | 2013-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb5b888091a0f0ca4f8622b54d45a267 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d10bd2cf99f3806795bef2c560d076b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_733ccb3037d61ee3863e29194841ffba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c0d87a831cc039739c4049c45c2c631 |
publicationDate | 2015-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103144178-B |
titleOfInvention | Production method of aldehyde-free bamboo floor |
abstract | The invention relates to a production method of an aldehyde-free bamboo floor, which comprises the following steps that firstly, modified soyabean albumen glue is prepared by components in parts by mass as follows: 100 parts of water, 5-60 parts of soybean albumen powder, 0.01-15 parts of a modifying agent, 0-5 parts of compound protease, 0-15 parts of a pH (potential of hydrogen) modifier, 0-15 parts of a viscosity modifier, 0.1-15 parts of an antiseptic mildew preventive, 0-10 parts of an auxiliary and 0-10 parts of a filler; secondly, the modified soyabean albumen glue is sheared to reduce viscosity by a mixer or a blending machine at the revolving speed of 50-300 revolutions per minute for 5 to 30 minutes; and thirdly, bamboo chips are used as a raw material and manufactured into the bamboo floor through processes of gluing, ageing, assembling and hot pressing. By means of the production method, free formaldehyde is absent, the environmental pollution is avoided, the environmental protection property is good, the water resisting property is good, and the gluing property is excellent. |