http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103137976-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 |
filingDate | 2011-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103137976-B |
titleOfInvention | Nano composite material and preparation method thereof and positive electrode and battery |
abstract | The invention provides a kind of nano composite material, described nano composite material comprises elemental lithium and transition metal, and wherein, described elemental lithium is from the oxide of lithium salts and/or lithium; Described transition metal is from the oxide of transition metal and/or transition metal; The mol ratio of described elemental lithium and transition metal is 0.25 ~ 8: 1, is preferably 1 ~ 4: 1.Present invention also offers the preparation method of described nano composite material, and comprise serondary lithium battery positive electrode and the serondary lithium battery of described nano composite material. |
priorityDate | 2011-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |