http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103132332-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_96db7f4800d6c0cede851fefc62a362b |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-28 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-50 |
filingDate | 2013-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_470eb83f2f3274cf298ce66967408088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b148c99e817b3925b4c06d255bfb19f1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f5953d58dff2adcd66c1a98ad4b9aeb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c4c6b81d41a6ee2c5234b1748cccc12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_33f7a2719ec7c670d603ab3dd85663ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c524251db220740a7f2709f16d76003 |
publicationDate | 2015-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103132332-B |
titleOfInvention | Fibrous material with formaldehyde removal function |
abstract | The invention discloses a fibrous material with a formaldehyde removal function, and belongs to the technical field of poisonous volatile matter removal. Cation exchange fibers are used as base body materials in the fibrous material, and counting the total mass of the fibrous material by 100%, the fibrous material comprises, by mass, 24.8%-88.95% of the cation exchange fiber, 0.05%-0.2% of surface active agent, and 11%-75% of macromolecule organic amine compound. The preparation method of the fibrous material includes the following steps: (1) preparing steeping liquor according to proportion, (2) adding fibers into the steeping liquor and evenly stirring the fibers, (3) soaking the fibers in the steeping liquor for 2-4 hours under the condition of interval stirring, (4) and fishing out the soaked materials, drying the materials with hot air or natural air. The fibrous material is diversified in application form, has no secondary pollution, and is large in formaldehyde adsorption capacity, high in adsorption speed, simple in preparation process, and low in cost. |
priorityDate | 2013-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links