classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2253-108 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G2300-405 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G2300-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P30-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2255-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G11-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G3-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G25-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-2803 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28057 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-3042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-186 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-3007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B37-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B39-48 |
filingDate | 2011-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103124694-B |
titleOfInvention | Zeolitic material of LEV type structure and preparation method thereof |
abstract | Provide zeolitic material of LEV type structure and preparation method thereof.Comprise YOn 2 and optionally comprise Xn 2 on 3 the preparation method with the zeolitic material of LEV type structure comprise the steps: (1) preparation comprise one or more YOn 2 source, one or more solvents and optionally comprise the mixture of seed crystal; (2) make the crystalline mixture of gained in step (1), wherein Y is quadrivalent element, and X is trivalent element, and described zeolitic material optionally comprises one or more basic metal M, one or more solvent total amounts described with YOn 2 one or more YO described of metern 2 the mol ratio of source total amount is 9.5 or less, and the Tc in step (2) is 175 ° of C or higher, and crystallization time is at these tem-peratures less than 14 days.Can according to or have comprise YO according to the described zeolitic material that the present invention obtainsn 2 and optionally comprise Xn 2 on 3 lEV type structure, one or more basic metal M and to demonstrate Y:X atomic ratio be 1-9.4. |
priorityDate | 2010-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |