http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103102531-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3a41f37239048502b51bbf174a273687 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-11 |
filingDate | 2012-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69e40e213330837ec3059588cd533116 |
publicationDate | 2015-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103102531-B |
titleOfInvention | Leather cup rubber for laundry machine and preparation method thereof |
abstract | The invention discloses leather cup rubber for a laundry machine. The leather cup rubber is prepared from the following raw materials in parts by weight: 30-40 parts of nitrile rubber, 20-30 parts of chlorosulfonated polyethylene rubber, 20-40 parts of ethylene propylene terpolymer 5962 (LANXESS Deutschland), 10-15 parts of fluorine rubber, 3-5 parts of natural rubber, 20-30 parts of high abrasion furnace black N330, 10-15 parts of modified white carbon black, 3-4 parts of zirconia, 8-10 parts of modified wood ash, 4-6 parts of attapulgite, 4-6 parts of meerschaum, 9-11 parts of modified iron tailing slag powder, 0.5-1 part of stearic acid, 0.5-1 part of isocyanate, 0.2-0.4 part of accelerant DM, 0.3-0.6 part of accelerant BZ, 1-2 parts of stearic acid, 2-4 parts of zinc oxide, 0.2-0.4 part of ferrocene, 1-2 parts of polyethylene wax, 1-2 parts of antioxidant DSTP, 1-2 parts of anti-aging agent NBC, 2-3 parts of gamma-methacryloxypropyl trimethoxysilane and 16-18 parts of triethyl citrate. The rubber disclosed by the invention has excellent ozone resistance, excellent low temperature resistance and heat resistance and is large in operating temperature range and environment-friendly in process, so that the rubber can be used for preparing various packing materials. |
priorityDate | 2012-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 80.