http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103058254-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_67ac1726fbb073d3deb088d6bb59dc21 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F17-00 |
filingDate | 2012-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-12-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82e0edec6fa8be66567bd1c6acdbec8b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14f4e5bc485d51c21420b645c7650e53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0990de0063863aea8a5aeb2edb1b7a21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8e8dcd1d7c7d500f1b1683251d6cb7cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2879e5f936eb17c3d40353c784a8a91e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0cd0529dc477021ab56394a298a4dda http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_47e42c1c706dbbec680a8d697d9af2a0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2549e56db4b3603f84e6b8efbb12b7cd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79c203ab64698a93f468a5ec8a1e9fa9 |
publicationDate | 2014-12-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103058254-B |
titleOfInvention | Preparation method of large-particle lutetium oxide |
abstract | The invention relates to a preparation method of large-particle lutetium oxide, belonging to a preparation technology of material. The method comprises the following steps of: preparing an ammonium bicarbonate solution with ammonium bicarbonate, ammonia water and deionized water, adding lutetium nitrate hydrate solution to the ammonium bicarbonate solution to obtain a mixed solution of ammonium bicarbonate, ammonia water and lutetium nitrate hydrate, adding hydrogen peroxide to the mixed solution, reacting for 6 hours to generate a lutetium carbonate hydrate precipitation, aging for 24-48 hours, filtering and washing the precipitation, keeping the firing temperature at 900-1200 DEG C for thermal insulation for 4 hours to obtain the large-particle gadolinium oxide product, which has the characteristics of uniform particle, favorable liquidity, and the morphology of which appears to be a petal piled by sheet and the central grain size D50 of which is 50-165 micrometers. |
priorityDate | 2012-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |