http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103046159-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c23d84d2f6dd5c06aea424c9fb3bc340 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-09 |
filingDate | 2012-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_540009fd531b580ec86177c92f468058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bea9bf5266f4da3f4de1a639c667ea0a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_be49db4482b3225d93e5b144dc043520 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_21c3131c50f79671341fb021382c8366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_95e79d584b3b08fe7deed1f1dc50d838 |
publicationDate | 2014-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103046159-B |
titleOfInvention | Manufacturing method of polyamide conductive fibres |
abstract | The invention discloses a manufacturing method of polyamide conductive fibres, which comprises the following steps of: A) uniformly mixing tetrapod-like zinc oxide whiskers and conductive potassium titanate whiskers, then calcining in a vacuum furnace; after cooling, stirring and dispersing by using sodium hexametaphosphate in anhydrous ethanol, then carrying out a plasma treatment at the normal temperature, carrying out ultrasonic dispersion and cleaning by reusing deionized water containing a calcium stearate dispersion liquid, taking solution upper suspension whiskers to be filtered by 150 meshes, taking a modified whisker mixed liquid, and repeating the operation until the filtration, drying in a vacuum oven after filtration to obtain a modified whisker mixture; B) stirring the modified whisker mixture obtained in the step A) with antimony-doped tin oxide conductive powder, superconducting super-conductive carbon black, a titanate coupling agent, an aluminate coupling agent and polyethylene wax in a mixer to obtain a modified whisker conductive comixture; C) blending and melting the modified whisker conductive comixture obtained in the step B) with polyamide powder, a PE-g-MAH phase flux and a 1010 antioxidant in the presence of trace sodium hexametaphosphate to be prepared into conductive polyamide slices; and D) preparing conductive polyamide and conventional polyamide to be sheath-core polyamide conductive fibers through a composite spinning technology. |
priorityDate | 2012-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |