http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103030828-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cc4e13141d402ceb885f368dfa042348 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-22 |
filingDate | 2012-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dbbf14b467e1c9307b1f1db939c2b2e6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a19cdc31a843c55f5d8843c7beb1f73e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c46d2ae7f7442c65c4f92bc308a1dc2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f02f040dab02d5f5f8fd7f719ae3466d |
publicationDate | 2014-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103030828-B |
titleOfInvention | Preparation method of rubber-based composite material with super-hydrophobic surface |
abstract | The invention discloses a preparation method of a rubber-based composite material with the super-hydrophobic surface. The preparation method comprises the following steps: firstly placing an aluminum sheet into chemical corrosive liquid to corrode for 2-120 minutes, washing the corroded aluminum sheet by deionized water, drying for standby; placing a mixed rubber compound onto the corroded aluminum sheet, then using a press vulcanizer to vulcanize or tablet the sheet; separating the cooled aluminum sheet from the rubber; brush coating an ethanol solution of a low surface energy substance on the rough surface of the separated rubber-based composite material, taking reaction for 1-36 hours at the temperature of 40-200 DEG C, and at last obtaining the rubber-based composite material with the micro-nano coarse structure super-hydrophobic surface. The surface water contact angle of the super-hydrophobic rubber-based composite material is more than 150 degrees; the rolling angle is smaller than 8 degrees; the super-hydrophobic rubber-based composite material has excellent comprehensive properties such as high elasticity, high abrasion resistance and high strength, is simple in preparation technology and beneficial to large-scale production and application. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105602052-A |
priorityDate | 2012-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 79.