http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103013331-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be2c55a9de09e08e3404c0a5a1ae4dc7 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-385 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 |
filingDate | 2013-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_279778603e95c0901832cacb9adf7f84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f159e6d52fe7a2b0ac793e5d015d0c47 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_74e201f23d6d86d8329cc4ad1345595e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_229928538bf5bda3a9ea8fb76a2e3087 |
publicationDate | 2015-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103013331-B |
titleOfInvention | Double-component fluorosilicone rubber ice-covering-proof coating material and preparation method thereof |
abstract | The invention discloses a double-component fluorosilicone rubber ice-covering-proof coating material and a preparation method thereof. The preparation method comprises the following steps: dissolving fluorine-containing acrylate in solvent, adding a platinum catalyst, uniformly stirring, and pouring into a four-neck flask; starting an electromagnetic stirrer, introducing inert gas, heating in water bath, adding hydrogen-containing silicone oil, and reacting to generate fluorine modified silicone oil; placing vinyl terminated polydimethylsiloxane in a beaker, adding 5-40 parts by mass of white carbon black used as reinforcement filler, evenly stirring, then adding 0.5-5 parts by mass of whitener TiO2, and evenly stirring; weighing 1-5 parts by mass of hydrogen-containing silicone oil and 1-5 parts by mass of fluorine modified silicone oil, placing in the beaker, evenly stirring, adding 10-50mu L of platinum catalyst, and finally adding the solvent; and evenly coating through a spin coater, and curing in a baking oven for 1-4 hours, thus obtaining the double-component fluorosilicone rubber coating. The invention overcomes the defects in the prior art, uses polyorganosiloxane as the raw material, can achieve satisfactory ice-covering-proof effect and is used in the fields of paint and the like. |
priorityDate | 2013-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 55.