http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103011701-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-00 |
filingDate | 2011-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103011701-B |
titleOfInvention | A kind of kervit microbead insulated sand slurry and preparation method thereof |
abstract | The invention provides a kind of kervit microbead insulated sand slurry; described kervit microbead insulated sand slurry comprises glass bead, cement, pre-gelatinized starch and gelatin; the content of described glass bead is 30 ~ 70 weight parts; the content of described cement is 20 ~ 40 weight parts; the content of described pre-gelatinized starch is 0.1 ~ 3 weight part, and the content of described gelatin is 0.1 ~ 2 weight part.Present invention also offers the preparation method of above-mentioned kervit microbead insulated sand slurry, comprise the steps: to take raw material in proportion, described raw material comprises glass bead, cement, pre-gelatinized starch and gelatin; After above-mentioned load weighted raw material stirring is even, obtain kervit microbead insulated sand slurry.Kervit microbead insulated sand slurry environmental protection of the present invention, cheaper starting materials are easy to get, and can effectively reduce costs, and have excellent resistance to cleavage and compressive property. |
priorityDate | 2011-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links