http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103004877-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fe23165b82e0c0988bab6c2beb449a00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N59-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01P1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01P3-00 |
filingDate | 2012-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1f1b1097f9589fdaf12ab7d07c37cea http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c890a0294d6ed48bfbcdf543d7b975e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_426e82023b0701aa5c977870836392bc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cdcd752912661f3f6862d772c550a293 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da8b12c44d5478f41cf0fda625d6a3cf |
publicationDate | 2015-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103004877-B |
titleOfInvention | Method for preparing silver-loaded titanate-zirconium phosphate composite nanometer material |
abstract | The invention discloses a method for preparing a silver-loaded titanate-zirconium phosphate composite nanometer material. The method comprises the steps of: firstly, adding titanate into deionized water to be dispersed, adding phosphoric acid; regulating pH using ammonia water, adding silver nitrate after uniform dispersion; stirring the resulting solution under a light-proof condition for 6-24 hours; adding an aqueous solution of zirconium salt, and further stirring the resulting solution under the light-proof condition for 2-8 hours; washing and drying a sediment product after the stirring operation is ended; and roasting the sediment product at the temperature of 500-1200 DEG C to obtain the target product silver-loaded titanate-zirconium phosphate composite nanometer material. The preparation method is simple and convenient in process and flow, wide in parameter adjustable range, strong in repeatability, low in cost, conductive to large-scale production, and has good business prospect. |
priorityDate | 2012-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 51.