http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102993853-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 |
filingDate | 2012-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102993853-B |
titleOfInvention | A kind of nontoxic material release type anti-fouling paint and preparation method thereof |
abstract | The present invention provides a kind of nontoxic material release type anti-fouling paint, and described anti-fouling paint includes: (a) first component includes by weight/mass percentage composition: fluorocarbon resin 38-48, organic siliconresin 13-22, dispersant 0.5-4, color stuffing 23-42, defoamer 0.2-0.6, levelling agent 0.2-0.6, solvent 6-12;Each component sum of described first component is 100%;The firming agent of (b) first constituent mass 2-8%.Nontoxic material release type anti-fouling paint provided by the invention can be main with organic-silicon-modified fluorocarbon resin for film forming matter, the in addition composition such as pigment, filler, auxiliary agent, by low-surface-energy, fine and smooth fine and close paint film, allow marine growth cannot be attached to its surface, even if having a small amount of sea organism attachment herein above, in ship navigation process, ship's speed is when 14-16 saves, due to its attachment loosely, self falling, thus reaching anti-fouling effect. |
priorityDate | 2012-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |