Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e0bf0928b608797b70bbc2b91c7e52e |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G81-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-916 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 |
filingDate |
2011-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fac57c0fadb0117cd7cef01ee792ea70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad81c96a6682be3d8aaa6094b2a331cc |
publicationDate |
2014-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-102971357-B |
titleOfInvention |
Method for increasing the molecular weight of polyesters |
abstract |
The invention relates to a method for increasing the molecular weight of polyesters by heating 100 parts of polyester with i) 0.01 to 5 parts of a tetracarbolic acid dianhydride, and ii) 0.01 to 5 parts of a copolymer comprising an epoxy group and based on styrene, acrylic acid ester, and/or methacrylic acid ester in an extruder to 160 to 350 DEG C. |