http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102935388-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e94fe056ef0d7f5177bb40c01d343bb8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J38-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J38-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J38-62 |
filingDate | 2012-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_603f92048a2578f90b7ba353f1234d29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ebb201f710ed21ed73ccfa3488bca74e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e95e4f549c3fd2572ac6fff767d55af4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7d279db1fe340b5cc5d00edafa870044 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6bf0a3e6ac3821690f763e5ffda41001 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98030d812b2f6455a652da76af4ed38b |
publicationDate | 2014-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102935388-B |
titleOfInvention | Antitoxic regeneration solution of deactivated SCR denitration catalyst, and preparation method thereof |
abstract | The invention relates to an antitoxic regeneration solution of a deactivated SCR denitration catalyst, and a preparation method thereof. The antitoxic regeneration solution comprises an active replenisher, an antitoxic modification liquid, and an additive component. The active replenisher comprises ammonium metavanadate, ammonium tungstate, and acid liquid. The antitoxic modification liquid comprises germanium nitrate, ammonium molybdate tetrahydrate, and ammonium cerium nitrate. The additive component comprises a penetrating agent, a dispersing agent, and an adhesive. According to the invention, the prepared active replenisher, antitoxic modification liquid, and additive component are well mixed according to a certain weight ratio, such that an antitoxic regeneration solution is obtained. The solution and the preparation method provided by the invention have the advantages that: the deactivated catalyst is pickled, and active components are simultaneously replenished, such that catalyst denitrification efficiency is recovered to above 90%. With the existence of the antitoxic component, the antitoxic performance of the catalyst is substantially improved, such that catalyst arsenic, sulfur and alkali metal toxic effects can be effectively relieved, and service life of the catalyst after regeneration is prolonged. |
priorityDate | 2012-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |