titleOfInvention | Anion-modified emulsified bitumen of a kind of Thief zone and preparation method thereof |
abstract | The invention provides anion-modified emulsified bitumen of a kind of Thief zone and preparation method thereof, its composition comprises pitch, thinner, emulsifying agent, permeate agent, water, stablizer and negatively charged ion SBR latex; Preparation process adopts colloidal mill emulsification to obtain the finished product by the proportioning and processing temperature controlling material; Prepared emulsified bitumen good stability, penetrating power are strong, and what can meet code requirement penetrates basic unit 5 ~ 10mm degree of depth; The present invention's thinner used be crude oil or petroleum fractionating extract rough residual oil, white oil, the light oil and other industrial byproducts of processing mixture, burning-point is high, volatility is little, cheap, preparation the environmental protection of Thief zone emulsified bitumen and cost is lower, and adopt composite emulsifying agent to improve emulsion property, the permeate agent adopted is preferred through relative permeate Force meansurement, improves the wicking capacity of product. |